Material Number | Material Number (single) | Standard | Range of Application | Standard Status | Country | Successor | Remark | Application temperature [°C] |
---|---|---|---|---|---|---|---|---|
1.4855 (DIN 17465 : 1993-08) | 1.4855 | DIN 17465 : 1993-08 | DIN 17465 : 1993-08 replaced by DIN EN 10295 : 2003-01 | Replaced | Germany | GX40CrNiSiNb24-24 | G-X 30 CrNiSiNb 24 24, for industry oven and natural gas systems resistance: - in carburising gas: good - in nitrogenous gas: good - in oxidising sulfureous gas: middle - in reductive sulfureous gas: low - temperature loading on air: up to 1050°C | ≤ 1050 |
Chemical Composition
C [%] | Cr [%] | Mn [%] | Nb [%] | Ni [%] | P [%] | S [%] | Si [%] | Source |
---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur |
Mechanical Properties
Semi-finished Product | Condition | Temperature [°C] | Tensile Strength [MPa] | Yield Strength (0.2% offset) [MPa] | Elongation A [%] | Source | Remark |
---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur |
Physical Properties
Temperature [°C] | Density [g/cm³] | Young's Modulus [GPa] | Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] | Thermal Conductivity [W/(m*K)] | Specific Electrical Resistance [µΩm] | Mean Specific Heat Capacity [kJ/(kg*K)] | Source |
---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur |
Young's Modulus [GPa] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowMean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowCreep Rupture Behaviour
Temperature [°C] | Creep Tensile Strength at 10^4 h [MPa] | Creep Tensile Strength at 10^5 h [MPa] | 1% Creep Limit at 10^4 h [MPa] | Source | Remark |
---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur |
Cross Reference
Material Name | Country |
---|---|
GX40CrNiSiNb24-24 | Germany |
GX30CrNiSiNb24-24 | Germany |
Producer/Supplier/Trade names
Tradename | Supplier |
---|---|
1.4855 | Klaus Kuhn Edelstahlgießerei GmbH, Radevormwald |
1.4855 | ZAPP AG, Ratingen |
1.4855 | SCHMOLZ + BICKENBACH GUSS GmbH, Krefeld |
A 1224 Nb | Otto Junker GmbH, Edelstahlgießerei, Simmerath |
Dux G 4855 | Swiss Steel International GmbH, Düsseldorf |
G 4855 | Dörrenberg Edelstahl GmbH, Engelskirchen |
Guronit 24 N 24 Nb | SCHMOLZ + BICKENBACH GUSS GmbH, Krefeld |
GX30CrNiSiNb24-24 | Pleissner Guss GmbH, Herzberg am Harz |
Märker G 4855 | Schmidt + Clemens GmbH + Co. KG, Edelstahlwerk Kaiserau, Lindlar |
PK 24 | Albert Hoffmann GmbH, Eschweiler |
Pyrotherm G 24/24 Nb | SCHMOLZ + BICKENBACH GUSS GmbH, Krefeld |
ZGN 24 Nb | Friedr. Lohmann GmbH, Witten |
Material Compliance
REACh | RoHS |
---|---|
blur | blur |