Cu-ETP1 | CW003A Material Datasheet - Properties - Materials Portal

Cu-ETP1 | CW003A Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access

Material Description

Material NumberMaterial Number (single)StandardRange of ApplicationStandard StatusCountryPredecessorRemark
CW003A (DIN EN 13605 : 2021-07) CW003A DIN EN 13605 : 2021-07Supersedes DIN EN 13605 : 2013-09ValidGermanyCu-ETP1Copper profiles and profiled wire for electrical purposes. Tough pitch copper (oxygencontaining coppers) of this type are produced with a controlled amount of oxygen and have high electrical conductivity. Special precautions are necessary when heat-treating, welding or brazing these coppers in atmospheres containing hydrogen to avoid hydrogen embrittlement.

Chemical Composition

Ag [%]As [%]Bi [%]Fe [%]O [%]Pb [%]S [%]Sb [%]Se [%]Te [%]SourceRemark
blurblurblurblurblurblurblurblurblurblurblurblur

Mechanical Properties

Semi-finished ProductConditionStrength AbbrevationNominal Size [mm]Temperature [°C]Tensile Strength [MPa]Yield Strength (0.2% offset) [MPa]Elongation A100 [%]Elongation A [%]Hardness HB | HBWHardness HVSource
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur

Physical Properties

ConditionStrength AbbrevationTemperature [°C]Specific Electrical Resistance [µΩm]Electric Conductivity [MS/m]Specific Mass Resistance [Ωg/m²]Specific Electric Conductivity [% IACS]Source
blurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblur

Welding and Joining

ProcedureWelding and Joining - EvaluationSource
blurblurblur
blurblurblur

Cross Reference

Material NameCountryStandardSource
T1ChinaGB/T 5231Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
Cu-ETP1EuropeEN 13605 
C 1020 WJapanJIS H 3260Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
M00RussiaGOST 859Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
B49 UNS C11040USAASTM B49Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
C11040USAUNSDeutsches Kupferinstitut Berufsverband e.V., Düsseldorf
E1-Cu58Germany Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
2.0061GermanyDIN 1708Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf

Producer/Supplier/Trade names

TradenameSupplier
CW003AAurubis Stolberg GmbH + Co. KG, Stolberg
CW003AFeindrahtwerk Adolf Edelhoff GmbH & Co, Iserlohn
CW003AOTTO BRENSCHEIDT GmbH & Co. KG, Sundern
CW003AKME Mansfeld GmbH, Hettstedt
CW003ASundwiger Messingwerk GmbH & Co.KG, Hemer

Material Compliance

REAChRoHS
blurblur

Cu-ETP1 (CW003A; DIN EN 13605 : 2021-07)

Linear-elastic

Temperature [°C]Young's modulus [GPa]Poisson's ratio
blurblurblur
blurblurblur

Yield strength

Temperature [°C]0.2% Proof strength [MPa]
blurblur

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

WIAM MaterialSource description
blurblur

Designation

DesignationMaterial numberSource
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur
blurblurblur


Cu-ETP1 (soft annealed (+A); 4mm; not specified)

Strain life

Temperature [°C]Cyclic fatigue strength coefficient [MPa]Cyclic fatigue strength exponentDuctility coefficient [Pa]Ductility exponentCyclic strength coefficient [MPa]Cyclic strain hardening exponentYoung's modulus [GPa]
blurblurblurblurblurblurblurblur

Classification

TreatmentDimension [mm]Failure criteriaSource description
blurblurblurblur


Cu-ETP1 (soft annealed (+A); 6.35mm; not specified)

Strain life

Temperature [°C]Cyclic fatigue strength coefficient [MPa]Cyclic fatigue strength exponentDuctility coefficient [Pa]Ductility exponentCyclic strength coefficient [MPa]Cyclic strain hardening exponentYoung's modulus [GPa]
blurblurblurblurblurblurblurblur

Classification

TreatmentDimension [mm]Failure criteriaSource description
blurblurblurblur


Cu-ETP1 (drawn)

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Classification

TreatmentSource description
blurblur


Cu-ETP1 (H035)

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Classification

TreatmentSource description
blurblur


Cu-ETP1 (R200)

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Classification

TreatmentSource description
blurblur


Cu-ETP1 (H065)

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Classification

TreatmentSource description
blurblur


Cu-ETP1 (R240)

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Classification

TreatmentSource description
blurblur


Cu-ETP1 (H080)

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Classification

TreatmentSource description
blurblur


Cu-ETP1 (R280)

Electrical resistivity

Temperature [°C]Specific electrical resistance [µΩm]
blurblur

Classification

TreatmentSource description
blurblur


Cu-ETP1 (soft annealed (+A); wire; 0.000-3.000mm)

Yield strength

Temperature [°C]0.2% Proof strength [MPa]
blurblur

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

TreatmentSemi-finished productDimension [mm]Source description
blurblurblurblur


Cu-ETP1 (soft annealed (+A); wire; 3.000-50.000mm)

Yield strength

Temperature [°C]0.2% Proof strength [MPa]
blurblur

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

TreatmentSemi-finished productDimension [mm]Source description
blurblurblurblur


Cu-ETP1 (R240; wire; 0.000-10.000mm)

Yield strength

Temperature [°C]0.2% Proof strength [MPa]
blurblur

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

TreatmentSemi-finished productDimension [mm]Source description
blurblurblurblur


Cu-ETP1 (R280; wire; 0.000-5.000mm)

Yield strength

Temperature [°C]0.2% Proof strength [MPa]
blurblur

Tensile strength

Temperature [°C]Tensile strength [MPa]
blurblur

Classification

TreatmentSemi-finished productDimension [mm]Source description
blurblurblurblur