GX40CrNiSi25-20 | 1.4848 Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access

Material Description

Material Number Material Name Material Number (single) Standard Scope Standard Status Country Successor VDA 231-106 classification Application temperature [°C]
1.4848 (DIN 17465 : 1993-08) GX40CrNiSi25-20 1.4848 DIN 17465 : 1993-08 DIN 17465 : 1993-08 replaced by DIN EN 10295 : 2003-01 Replaced Germany GX40CrNiSi25-20 1.1.2 ≤ 1150 1)
1) Remark: G-X 40 CrNiSi 25 20, for parts of ovens with highest mechanical loadings, previously loaded to high heat resistance, like transport elements in oven for annealing, tempering, sheet normalising and throughput, this are for example rolls, bearing arbor, bearing grate, bolts, anchor, lever, oven plates, burner, chains, snail retorts, transport rolls. Furthermore for insert boxes, annealing boxes, mortar trough, annealing hood, saucer, caps, burn roods and bearing stator. resistance: - in oxidising burning atmosphere: 1150°C - in reductive burning atmosphere: sensitive for carborising, especially upper 900°C - in oxidising sulfureous gas: in limited case - in reductive sulfureous gas: unresistant

Chemical Composition

C [%] Cr [%] Mn [%] Ni [%] P [%] S [%] Si [%] Remainder
blur blur blur blur blur blur blur blur 1)
1) Source: blur

Material Compliance

REACh RoHS
blur blur

Mechanical Properties

Semi-finished Product Condition Temperature [°C] Tensile Strength [MPa] Yield Strength (0.2% offset) [MPa] Elongation A [%]
blur blur blur blur blur blur 1)2)
1) Source: blur
2) Remark: blur

Physical Properties

Temperature [°C] Density [g/cm³] Young's Modulus [GPa] Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] Thermal Conductivity [W/(m*K)] Specific Electrical Resistance [µΩm] Mean Specific Heat Capacity [kJ/(kg*K)]
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 2)
blur blur blur blur blur blur blur 2)
blur blur blur blur blur blur blur 2)
blur blur blur blur blur blur blur 2)
blur blur blur blur blur blur blur 2)
1) Source: blur
2) Source: blur

Creep Rupture Behaviour

Temperature [°C] Creep Tensile Strength at 10^4 h [MPa] Creep Tensile Strength at 10^5 h [MPa] 1% Creep Limit at 10^4 h [MPa]
blur blur blur blur 1)2)
blur blur blur blur 1)2)
blur blur blur blur 1)2)
blur blur blur blur 1)2)
blur blur blur blur 2)3)
blur blur blur blur 2)3)
blur blur blur blur 2)3)
blur blur blur blur 2)3)
blur blur blur blur 2)4)
blur blur blur blur 2)4)
blur blur blur blur 2)4)
blur blur blur blur 2)4)
1) Source: blur
2) Remark: blur
3) Source: blur
4) Source: blur

Cross Reference

Material Name Country Standard
422952 Czech Republik/Slovakia CSN 422952
GX40CrNiSi25-20 Germany SEW 595
310C40 Great Britain BS 1504-76
310C40 Great Britain BS 3100-91
310C45 Great Britain BS 3100-91
G X 40 CrNi 26 20 Italy UNI 3159-83
SCH 21 Japan JIS G 5122-87
SCH 22 Japan JIS G 5122-87
F.8452-AM-X 40 CrNi 25 20 Spain UNE 36258-74
40CrNiSi2520 Hungary MSZ 4357
HK USA ASTM A 297