50 CrV 4 | 1.8159 Material Datasheet
Unlock Exclusive Materials Data
Gain access to a wealth of materials data by joining our Materials Portal.
Register for Free or Upgrade for Full AccessMaterial Description
Material Number | Material Number (single) | Standard | Range of Application | Standard Status | Country | Successor | Remark | Application temperature [°C] |
---|---|---|---|---|---|---|---|---|
1.8159 (DIN 1652-4 : 1990-11) | 1.8159 | DIN 1652-4 : 1990-11 | DIN 1652-4 : 1990-11 replaced by DIN EN 10277-5 : 1999-10 | Replaced | Germany | 51CrV4 | Steel 50 CrV 4 is suitable for high loaded parts that have to meet increased tempering and high wear resistance requirements at best core qualities in aircraft and vehicle construction and engine and machine engineering (e.g. transmission and joint parts, axles). Furthermore application to spring and tool steel. Lowest application temp. -25 °C. | ≥ -25 |
Chemical Composition
C [%] | Cr [%] | Mn [%] | P [%] | S [%] | Si [%] | V [%] | Source |
---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur |
Mechanical Properties
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Tensile Strength [MPa] | Yield Strength [MPa] | Elongation A [%] | Reduction of Area [%] | Hardness HB | HBW | Source | Remark |
---|---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Physical Properties
Temperature [°C] | Density [g/cm³] | Young's Modulus [GPa] | Poisson's Ratio | Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] | Differential Coefficient of Thermal Expansion [10^-6*K^-1] | Thermal Conductivity [W/(m*K)] | Thermal Diffusivity [10^-6 m²/s] | Specific Electrical Resistance [µΩm] | Mean Specific Heat Capacity [kJ/(kg*K)] | True Specific Heat Capacity [kJ/(kg*K)] | Source | Remark |
---|---|---|---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Young's Modulus [GPa] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowMean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowDifferential Coefficient of Thermal Expansion [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowToughness Data (Impact)
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Specimen Shape | Notch Impact Energy [J] | Source | Remark |
---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur |
Cross Reference
Material Name | Country | Standard |
---|---|---|
50 CrV 4 | Belgium | NBN 253-05 |
50CrVA | China | GB 3077 |
50 CV 4 | France | NF A 35-552 |
735 A 50 | Great Britain | BS 970/2 |
50 ChFA | Russia | GOST 14959 |
51 CrV 4 | International | ISO 683/1-87 |
50 CrV 4 | Italy | UNI 7845 |
SUP 10 | Japan | JIS G 4101 |
50 Hf | Poland | PN H 84032 |
2230 | Sweden | MNC 852 E |
F.1430-51 CrV 4 | Spain | UNE 36-015 |
6150 | USA | ASTM A 322 |
51CrV4 | Germany | DIN EN 10277-5 |
Producer/Supplier/Trade names
Tradename | Supplier |
---|---|
50 CrV 4 | HEINE + BEISSWENGER Stiftung + Co.KG, Fellbach |
Material Compliance
REACh | RoHS |
---|---|
blur | blur |
50 CrV 4 (1.8159; DIN 1652-4 : 1990-11)
Linear-elastic
Temperature [°C] | Young's modulus [GPa] | Poisson's ratio |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
Alternating stress
Temperature [°C] | Stress ratio | Alternating stress [MPa] | Cycles |
---|---|---|---|
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Electrical resistivity
Temperature [°C] | Specific electrical resistance [µΩm] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Coefficient thermal expansion
Related Temperature [°C] | Temperature [°C] | Coefficient thermal expansion [10^-6*K^-1] |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
Specific heat
Temperature [°C] | Specific heat [kJ/(kg*K)] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Density
Temperature [°C] | Density [g/cm³] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Thermal conductivity
Temperature [°C] | Thermal conductivity [W/(m*K)] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Classification
WIAM Material | Source description |
---|---|
blur | blur |
Designation
Designation | Material number | Source |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
50 CrV 4 (cold drawn or turned and quenched and tempered; bright steel; 0.000-16.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
50 CrV 4 (cold drawn or turned and quenched and tempered; bright steel; 16.000-40.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
50 CrV 4 (cold drawn or turned and quenched and tempered; bright steel; 40.000-80.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
50 CrV 4 (cold drawn; bright steel; 0.000-16.000mm)
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
50 CrV 4 (cold drawn; bright steel; 16.000-40.000mm)
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
50 CrV 4 (cold drawn; bright steel; 40.000-80.000mm)
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |