C 22 | 1.0402 Material Datasheet
Unlock Exclusive Materials Data
Gain access to a wealth of materials data by joining our Materials Portal.
Register for Free or Upgrade for Full AccessMaterial Description
Material Number | Material Number (single) | Standard | Range of Application | Standard Status | Country | Remark | Application temperature [°C] |
---|---|---|---|---|---|---|---|
1.0402 (DIN 1652-4 : 1990-11) | 1.0402 | DIN 1652-4 : 1990-11 | DIN 1652-4 : 1990-11 replaced by DIN EN 10277-5 : 1999-10 | Replaced | Germany | Steel C 22 is suitable for low strained parts of small heat treatment sections in vehicle manufacturing and machine engineering (e.g. piston-rods, gear wheels). Lowest application temperature -25 °C. | ≥ -25 |
Chemical Composition
C [%] | Mn [%] | P [%] | S [%] | Si [%] | Source |
---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur |
Mechanical Properties
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Tensile Strength [MPa] | Yield Strength [MPa] | Elongation A [%] | Reduction of Area [%] | Source | Remark |
---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Physical Properties
Temperature [°C] | Density [g/cm³] | Young's Modulus [GPa] | Shear Modulus [GPa] | Poisson's Ratio | Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] | Differential Coefficient of Thermal Expansion [10^-6*K^-1] | Thermal Conductivity [W/(m*K)] | Thermal Diffusivity [10^-6 m²/s] | Specific Electrical Resistance [µΩm] | Mean Specific Heat Capacity [kJ/(kg*K)] | True Specific Heat Capacity [kJ/(kg*K)] | Source | Remark |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Young's Modulus [GPa] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowMean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowDifferential Coefficient of Thermal Expansion [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowToughness Data (Impact)
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Specimen Shape | Notch Impact Energy [J] | Source | Remark |
---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur |
Cross Reference
Material Name | Country | Standard |
---|---|---|
AF42C20 | France | NF A 35-552 |
070 M 20 | Great Britain | BS 970/1 |
20 | Russia | GOST 1050 |
C 20 | Italy | UNI 7874 |
S 25 C | Japan | JIS G 4051 |
20 | Poland | PN H-84019 |
1020 | USA | ASTM A 576 |
Producer/Supplier/Trade names
Tradename | Supplier |
---|---|
C 22 | HEINE + BEISSWENGER Stiftung + Co.KG, Fellbach |
Material Compliance
REACh | RoHS |
---|---|
blur | blur |
C 22 (1.0402; DIN 1652-4 : 1990-11)
Linear-elastic
Temperature [°C] | Young's modulus [GPa] | Shear modulus [GPa] | Poisson's ratio |
---|---|---|---|
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
Alternating stress
Temperature [°C] | Stress ratio | Alternating stress [MPa] | Cycles |
---|---|---|---|
blur | blur | blur | blur |
blur | blur | blur | blur |
blur | blur | blur | blur |
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Electrical resistivity
Temperature [°C] | Specific electrical resistance [µΩm] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Coefficient thermal expansion
Related Temperature [°C] | Temperature [°C] | Coefficient thermal expansion [10^-6*K^-1] |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
Specific heat
Temperature [°C] | Specific heat [kJ/(kg*K)] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Density
Temperature [°C] | Density [g/cm³] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Thermal conductivity
Temperature [°C] | Thermal conductivity [W/(m*K)] |
---|---|
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
blur | blur |
Classification
WIAM Material | Source description |
---|---|
blur | blur |
Designation
Designation | Material number | Source |
---|---|---|
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
blur | blur | blur |
C 22 (sheet; 6.35mm; not specified)
Strain life
Temperature [°C] | Cyclic fatigue strength coefficient [MPa] | Cyclic fatigue strength exponent | Ductility coefficient [Pa] | Ductility exponent | Cyclic strength coefficient [MPa] | Cyclic strain hardening exponent | Young's modulus [GPa] |
---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur |
Classification
Semi-finished product | Dimension [mm] | Failure criteria | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn; bright steel; 0.000-5.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn; bright steel; 5.000-10.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn; bright steel; 10.000-16.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn; bright steel; 16.000-25.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn; bright steel; 25.000-40.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn; bright steel; 40.000-100.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn or turned and normalized; bright steel; 0.000-16.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn or turned and normalized; bright steel; 16.000-100.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn or turned and quenched and tempered; bright steel; 0.000-16.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |
C 22 (cold drawn or turned and quenched and tempered; bright steel; 16.000-40.000mm)
Yield strength
Temperature [°C] | Yield strength [MPa] |
---|---|
blur | blur |
Tensile strength
Temperature [°C] | Tensile strength [MPa] |
---|---|
blur | blur |
Classification
Treatment | Semi-finished product | Dimension [mm] | Source description |
---|---|---|---|
blur | blur | blur | blur |