GX40CrNiSi27-4 | 1.4823 Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access Best value

Material Description

Material Number Material Name Material Number (single) Standard Scope Standard Status Country Predecessor VDA 231-106 classification Application temperature [°C]
1.4823 (DIN EN 10295 : 2003-01) GX40CrNiSi27-4 1.4823 DIN EN 10295 : 2003-01 Supersedes DIN 17465 : 1993-08 Valid Germany GX40CrNiSi27-4 1.1.2 ≤ 1100 1)
1) Remark: According to DIN EN 10295 : 2003-01, the highest application temperature in air is 1100 °C for the material GX40CrNiSi27-4, material number 1.4823 (the former G-X 40 CrNiSi 27 4 according to DIN 17465 : 1977-09). The following is valid for the comparable DIN-material: Application for heat-resistant castings, e.g. movable furnace parts and firing parts, gate valves, rails, rolls, burner nozzles, moulds for glass. Also especially suitable for furnace parts that, under higher stress, are meant to be still resistant to gases containing sulphur, such as superheater mountings, tong-type drifts, annealing retorts and similar parts. Durability: - with an oxidizing combustion atmosphere: 1100 °C, - with a reducing combustion atmosphere: 1100 °C, - with oxidizing gases containing sulphur: 1100 °C, - with reducing gases containing sulphur: up to 1080 °C.

Chemical Composition

C [%] Cr [%] Mn [%] Mo [%] Ni [%] P [%] S [%] Si [%] Remainder
blur blur blur blur blur blur blur blur blur 1)2)
1) Source: blur
2) Remark: blur

Material Compliance

REACh RoHS
blur blur

Mechanical Properties

Semi-finished Product Condition Temperature [°C] Tensile Strength [MPa] Yield Strength (0.2% offset) [MPa] Elongation A [%]
blur blur blur blur blur blur 1)2)
1) Source: blur
2) Remark: blur

Physical Properties

Temperature [°C] Density [g/cm³] Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] Thermal Conductivity [W/(m*K)] Mean Specific Heat Capacity [kJ/(kg*K)]
blur blur blur blur 1)
blur blur 1)
blur blur 1)
blur blur blur 1)
blur blur blur 1)
1) Source: blur

Creep Rupture Behaviour

Temperature [°C] Creep Tensile Strength at 10² h [MPa] Creep Tensile Strength at 10³ h [MPa] 1% Creep Limit at 10^4 h [MPa]
blur blur blur blur 1)2)
blur blur blur 1)2)
blur blur blur 1)2)
blur blur blur blur 1)2)
blur blur 1)2)
1) Source: blur
2) Remark: blur

Cross Reference

Material Name Country Standard
ZG40Cr22Ni4N China GB/T 6403 1)
C53891 China GB/T 6403 1)
ZG40Cr22Ni4N China GB/T 8492 1)
C54890 China GB/T 8492 1)
GX40CrNiSi27-4 Europe EN 10295
4 (IS 4522) India IS 4522 1)
GX40CrNiSi27-4 International ISO 11973 1)
SCH11X Japan JIS G 5122 1)
A297 Grade HD USA ASTM A297 2)
HD USA ASTM A297 2)
Grade HD USA ASTM A297 2)
J93005 USA UNS 2)
GX40CrNiSi27-4 Germany DIN 17465
1) Source: Stahlschlüssel 2016, Verlag Stahlschlüssel Wegst GmbH, Marbach
2) Source: Metals & Alloys in the Unified Numbering System, SAE/ASTM, 11th Edition, 2008