GTW-40-05 | 0.8040 Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access

Material Description

Material Number Material Number (single) Standard Range of Application Standard Status Country Successor
0.8040 (DIN 1692 : 1982-01) 0.8040 DIN 1692 : 1982-01 DIN 1692 : 1982-01 replaced by DIN EN 1562 : 2006-08 Replaced Germany EN-GJMW-400-5 1)
1) Remark: GTW-40-05, decarburizing annealed malleable cast iron Application: for exhaust manifold, agricultural machinery parts, fittings, clutch parts (clutch catch muzzle), transmission case, bicycle parts, steering housings.

Chemical Composition

C [%] Mn [%] S [%] Si [%]
blur blur blur blur 1)2)
1) Source: blur
2) Remark: blur

Mechanical Properties

Semi-finished Product Condition Temperature [°C] Tensile Strength [MPa] Yield Strength [MPa] Elongation A [%] Hardness HB | HBW
blur blur blur blur blur blur blur 1)2)
blur blur blur blur blur blur blur 1)3)
blur blur blur blur blur blur blur 1)4)
1) Source: blur
2) Remark: blur
3) Remark: blur
4) Remark: blur

Cross Reference

Material Name Country Standard
MB 400-5 France NF A 32-701
W40-05 Great Britain BS 6681
W 40-05 International ISO 5922
W 40-05 Italy UNI ISO 5922
FCMW 370 Japan JIS G 5703
Type A Spain UNE 36113
EN-GJMW-400-5 (EN-JM1030) Germany DIN EN 1562

Producer/Supplier/Trade names

Material Compliance

REACh RoHS
blur blur

FKM Guideline Fatigue Strength

Semi-finished Product Condition Nominal Size [mm] Tensile Strength [MPa] Yield Strength (0.2% offset) [MPa] Elongation A3 [%] Fatigue Limit under rev. Tension-Compression Stresses [MPa] Fatigue Strength under pulsating Tensile Stresses [MPa] Bending Fatigue Strength [MPa] Shear Fatigue Strength [MPa] Torsion Fatigue Strength [MPa]
blur blur blur blur blur blur blur blur blur blur blur 1)2)
1) Source: blur
2) Remark: blur