G-CuSn6ZnNi | 2.1093 Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access Best value

Material Description

Material Number Material Name Material Number (single) Standard Scope Standard Status Country Successor VDA 231-106 classification
2.1093 (DIN 1705 : 1981-11) G-CuSn6ZnNi 2.1093 DIN 1705 : 1981-11 DIN 1705 : 1981-11 replaced by DIN EN 1982 : 1998-12 Replaced Germany CuSn7Zn2Pb3-C 3.2 1)
1) Remark: G-CuSn6ZnNi is a construction material with good strength and strains. It is resistant against sea water. It is used in machine engineering for armatures and pump casings as well as castings, with high demands on pressure safety. It is comparable with the strength properties of G-CuSn10Zn (2.1086, Rg10) Machining properties: Grindability: good Soft soldering: good Hard soldering: good Gas fusion welding: restricted Gas-shielding welding: poor Grindability (mech): good Galvanisability: good Immersing tin-plating: good

Chemical Composition

Cu [%] Fe [%] Ni [%] P [%] Pb [%] S [%] Sb [%] Sn [%] Zn [%]
blur blur blur blur blur blur blur blur blur 1)2)
1) Source: blur
2) Remark: blur

Material Compliance

REACh RoHS
blur blur 1)
1) Remark: blur

Mechanical Properties

Casting Method Condition Condition Number Temperature [°C] Tensile Strength [MPa] Yield Strength (0.2% offset) [MPa] Elongation A [%] Hardness HB | HBW
blur blur blur blur blur blur blur blur 1)
blur blur blur blur 1)
blur blur blur blur 1)
blur blur blur blur 1)
blur blur blur blur 1)
blur blur blur blur 1)
1) Source: blur

Physical Properties

Temperature [°C] Melting Temperature [°C] Density [g/cm³] Young's Modulus [GPa] Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] Thermal Conductivity [W/(m*K)] Linear Shrinkage [%] Electric Conductivity [MS/m]
blur blur blur blur blur blur 1)
blur blur 1)
blur 1)
1) Source: blur

Creep Rupture Behaviour

Temperature [°C] 0.1% Creep Limit at 10^4 h [MPa]
blur blur 1)
blur blur 1)
1) Source: blur

Cross Reference

Material Name Country Standard
CuSn7Zn2Pb3-C (CC492K) Germany DIN EN 1982

Producer/Supplier/Trade names

Tradename Supplier
Bögra Rotguß Rg6 BÖGRA Technologie GmbH, Solingen
G-CuSn6ZnNi CUMSAL GmbH, Wilnsdorf
G-CuSn6ZnNi Fehrmann Metallverarbeitung GmbH, Hamburg

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur

Density

Temperature [°C] Density [g/cm³]
blur blur

Linear-elastic

Temperature [°C] Young's modulus [GPa] Bulk modulus [GPa] Shear modulus [GPa] Poisson's ratio
blur blur
blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur
blur blur
blur blur
blur blur
blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur
blur blur
blur blur
blur blur
blur blur

Coefficient thermal expansion

Related Temperature [°C] Temperature [°C] Coefficient thermal expansion [10^-6*K^-1]
blur blur blur

Thermal conductivity

Temperature [°C] Thermal conductivity [W/(m*K)]
blur blur

Designation

Designation Material number Source
blur blur blur
blur blur
blur blur
blur blur
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur
blur blur
blur blur
blur blur
blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur
blur blur
blur blur
blur blur
blur blur
Diagram Settings

Diagram Preview
Select properties and click "Preview Diagram"