CuNi2 | 2.0802 Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access

Material Description

Material Number Material Name Material Number (single) Standard Standard Status Country VDA 231-106 classification Application temperature [°C]
2.0802 (DIN 17471 : 1983-04) CuNi2 2.0802 DIN 17471 : 1983-04 Valid Germany 3.2 ≤ 300 1)
1) Remark: CuNi2 is a resistance alloy. With wire, the attainable tensile strength is 220 N/mm². The resistivity is very low. The resistance to atmospheric corrosion is high. The upper application temperature in air is 300 °C. CuNi2 is of good suitability for soft soldering. Application: Terminal studs, low-ohm electric resistors, heater wires, heater cables with low heating temperature.

Chemical Composition

Ni [%] Remainder
blur blur 1)2)
1) Source: blur
2) Remark: blur

Material Compliance

REACh RoHS
blur blur

Mechanical Properties

Semi-finished Product Condition Nominal Size [mm] Temperature [°C] Tensile Strength [MPa] Elongation A100 [%]
blur blur blur blur blur blur 1)2)
blur blur blur blur blur blur 1)2)
blur blur blur blur blur blur 1)
blur blur blur blur blur blur 1)3)
1) Source: blur
2) Remark: blur
3) Remark: blur

Physical Properties

Temperature [°C] Melting Temperature [°C] Density [g/cm³] Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] Thermal Conductivity [W/(m*K)] Specific Electrical Resistance [µΩm] Mean Specific Heat Capacity [kJ/(kg*K)]
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
1) Source: blur

Producer/Supplier/Trade names

Tradename Supplier
Legierung 30 Isabellenhütte Heusler GmbH & Co.KG, Dillenburg