Material Number Material Number (single) Standard Scope Standard Status Country VDA 231-106 classification
1.0996 (DIN EN 10346 : 2015-10) 1.0996 DIN EN 10346 : 2015-10 Supersedes DIN EN 10346 : 2009-07 Valid Germany 1.1 1)
1) Remark: The cold-rolled dual phase steel HCT590X is a steel for cold forming with a minimum tensile strength of 590 N/mm².

Chemical Composition

Al [%] B [%] C [%] Mn [%] P [%] S [%] Si [%] V [%] Cr+Mo [%] Nb+Ti [%]
blur blur blur blur blur blur blur blur blur blur 1)
1) Source: blur

Mechanical Properties

Semi-finished Product Condition Nominal Size [mm] Temperature [°C] Specimen Direction Tensile Strength [MPa] Yield Strength (0.2% offset) [MPa] Elongation A80 [%] Bake-Hardening-Index [MPa] Strain Hardening Exponent n10-20/UE
blur blur blur blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur blur blur blur 1)
1) Source: blur

Welding and Joining

Welding and Joining - Evaluation
blur 1)
1) Source: blur

Cross Reference

Material Name Country Standard
HCT590X Europe EN 10346 1)
CR330Y590T-DP Germany VDA 239-100 2)
1) Source: Stahlschlüssel 2016, Verlag Stahlschlüssel Wegst GmbH, Marbach
2) Source: ArcelorMittal, Dualphasenstähle, 2018

Producer/Supplier/Trade names

Tradename Supplier
HCT590X Salzgitter Flachstahl GmbH, Salzgitter
HCT590X ThyssenKrupp Steel Europe AG, Duisburg

Material Compliance

REACh RoHS
blur blur

Linear-elastic

Temperature [°C] Young's modulus [GPa] Bulk modulus [GPa] Shear modulus [GPa] Poisson's ratio
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur

Alternating stress

Temperature [°C] Stress ratio Mean stress [MPa] Alternating stress [MPa] Cycles
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur blur blur blur blur blur blur blur blur

Designation

Designation Material number Source
blur blur blur
blur blur blur
blur blur blur
blur blur blur
blur blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur blur blur blur blur blur blur blur blur