E470 | 1.0536 Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access

Material Description

Material Number Material Number (single) Standard Standard Status Country
1.0536 (DIN EN 10294-1 : 2005-12) 1.0536 DIN EN 10294-1 : 2005-12 Valid Germany 1)
1) Remark: Seamless steel hollow bar intended for the manufacture of engineering components by machining.

Chemical Composition

Al [%] C [%] Mn [%] N [%] Nb [%] P [%] S [%] Si [%] V [%]
blur blur blur blur blur blur blur blur blur 1)
1) Source: blur

Mechanical Properties

Semi-finished Product Nominal Size [mm] Temperature [°C] Specimen Direction Tensile Strength [MPa] Yield Strength [MPa] Elongation A [%]
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
blur blur blur blur blur blur blur 1)
1) Source: blur

Cross Reference

Material Name Country Standard
E470 Europe EN 10294-1

Producer/Supplier/Trade names

Tradename Supplier
MecaPlus 470 Vallourec Deutschland GmbH, Düsseldorf
Ovako 280 OVAKO STAHL GmbH, Erkrath

Material Compliance

REACh RoHS
blur blur

Linear-elastic

Temperature [°C] Young's modulus [GPa] Bulk modulus [GPa] Shear modulus [GPa] Poisson's ratio
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur

Alternating stress

Temperature [°C] Stress ratio Mean stress [MPa] Alternating stress [MPa] Cycles
blur blur blur blur blur
blur blur blur blur blur
blur blur blur blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur blur blur blur blur blur blur blur blur

Designation

Designation Material number Source
blur blur blur
blur blur blur
blur blur blur
blur blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur blur blur blur blur blur blur blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur blur blur blur blur blur blur blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur blur blur blur blur blur blur blur blur

Yield strength

Temperature [°C] 0.1% Proof strength [MPa] 0.2% Proof strength [MPa] Yield strength [MPa]
blur blur blur blur

Tensile strength

Temperature [°C] Tensile strength [MPa]
blur blur

Classification

WIAM Material Treatment Semi-finished product Dimension [mm] Load type Failure criteria Rolling direction Maximum stress [MPa] Strain at maximum stress [%] Source description
blur blur blur blur blur blur blur blur blur blur